Macro and micro structural responses of dissimilar TC4/TC17 titanium alloy joints in linear friction welding and post-welding heat treatment processes and their effects on tensile and fatigue performance
The heterogeneous TC4 (Ti–6Al–4V)/TC17 (Ti–5Al–2Sn–2Zr–4Mo–4Cr) joint, formed by linear friction welding (LFW) and post-weld treatment, shows significant potential for blisk manufacturing in aircraft engines. Both LFW and heat treatment involve numerous parameters that can substantially impact joint...
Saved in:
| Main Authors: | , , , , , |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Elsevier
2025-07-01
|
| Series: | Journal of Materials Research and Technology |
| Subjects: | |
| Online Access: | http://www.sciencedirect.com/science/article/pii/S2238785425014711 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|