Synthesis of ultrafine (Mo,W)Si2 composite powders from high purity molybdenum concentrate

(Mo,W)Si2 composite powders with the grain size of about 1 μm were synthesized at 1150℃ for 2 h. The high purity molybdenum concentrate (with the main component of MoS2), W and Si powders were utilized as raw materials and lime as desulfurizer. The graphite felt was laid between the compact (made of...