Fracture Initiation in Aluminum Alloys Under Multiaxial Loading at Various Low Strain Rates

The initiation of ductile fractures in medium-strength AW5754 and high-strength AW6082 aluminum alloys at different quasi-static strain rates and under multiaxial stress states was investigated through a series of tensile tests using various specimen geometries. The sensitivity of the stress triaxia...