DECREASE OF BREAKAGE OF HIGH-STRENGTH WIRE AT METAL CORD TWIST ON MACHINES OF DOUBLE TORSION
Researches of the most often occurred surface defects of rolled wires, their modification at drawing and influence on technological process and quality of cold-drawn wire with regard to working conditions of hardware shops of BMZ are presented
Saved in:
Main Authors: | B. A. Biryukov, Yu. V. Feoktistov, A. V. Vedeneyev |
---|---|
Format: | Article |
Language: | English |
Published: |
Belarusian National Technical University
2012-11-01
|
Series: | Литьë и металлургия |
Online Access: | https://lim.bntu.by/jour/article/view/278 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
DEPENDENCE FOR CALCULATION OF METAL CORD BREAKAGE IN THE PROCESS OF SPIN ON WIRE SAWS OF DOUBLE TORSION
by: Yu. L. Bobarikin, et al.
Published: (2014-07-01) -
PROBLEMS OF WIRES MIGRATION OF INLAYS OF METAL CORD OF COMPACT STRUCTURES
by: A. V. Vedeneyev, et al.
Published: (2012-11-01) -
PROBLEMS OF MIGRATION OF WIRES OF THE METAL CORD INSIDE LAYERS OF COMPACT CONSTRUCTIONS
by: A. V. Vedeneev, et al.
Published: (2012-02-01) -
The Generalized Twist for the Torsion of Piezoelectric Cylinders
by: István Ecsedi, et al.
Published: (2017-01-01) -
WIRE BREAKAGE DURING WIRE DRAWING DUE TO THE PRESENCE OF SURFACE DEFECTS, INHERITED FROM WIRE ROD
by: A. S. Siarohina
Published: (2018-01-01)