Effects of diamond surface modification and matrix alloying on the thermal conductivity of copper/diamond composites

Diamond particles were roughened with Pr6O11 as the etching agent, and the diamond/copper (boron) composites with the diamond volume fraction of 60.0% and the boron volume fraction of 0.3% were prepared by spark plasma sintering. The effects of diamond surface modification and matrix boron alloying...