PECULIARITIES OF STRUCTURE FORMATION OF THE CONSTRUCTIONAL ALLOYED STEEL AT HEAT TREAT MENT OF HIGHQUALITY ROLLED IRON
The structure formation in electric steel 42Cr4Mo2 under continuous cooling is investigated, the results are summarized in the form of the thermo-kinetic diagram. It is shown that rolled metal annealing during 3.5-4.0 hours at 650-680°C provides the necessary properties of steel and enables to maint...