Round and pleated blisters: interface delamination in thin film deposition
Electron beam deposition is widely used in microelectronics manufacturing due to its ability to fabricate high-purity thin films at elevated rates. However, the formation of blisters during this process – resulting from delamination between the film and substrate – can compromise film integrity and...
Saved in:
| Main Authors: | Wenxiang Wang, Shengyao Chen, Jiacong Cao, Xiaoding Wei, Zhaohe Dai |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Taylor & Francis Group
2025-04-01
|
| Series: | International Journal of Smart and Nano Materials |
| Subjects: | |
| Online Access: | https://www.tandfonline.com/doi/10.1080/19475411.2025.2493663 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Pre-operative management of fracture blisters: a systematic review
by: Ishtar Redman, et al.
Published: (2025-03-01) -
Beyond the surface: Orthopaedic blister management “A review of the literature”
by: Amanda O'Halloran, et al.
Published: (2025-03-01) -
Localized genital blisters in an elderly male
by: An Jian Leung, MBBS, MRCP, MMed, et al.
Published: (2025-05-01) -
Massive Hemorrhagic Blisters following Bilateral Total Knee Replacement: A Case Report
by: Dhinesh Nadarajan Latha, et al.
Published: (2025-08-01) -
Internal Carotid Artery Blister Aneurysm: Review of Endovascular Techniques
by: Vipul Gupta, et al.
Published: (2021-04-01)