Coating stability of different esthetic NiTi archwires under high fluoride exposure
Methods: Ninety 0.016-inch esthetic nickel-titanium (NiTi) archwires were divided into three groups based on the type of coating (n=30): Group 1, rhodium-coated; Group 2, Teflon-coated; and Group 3, epoxy-coated. Each group was divided into three subgroups and kept in the following medium (n=10): A,...