The use of ATR-FTIR to track the degradation of single-use polystyrene cup lids during 24 months of temperate outdoor exposure.

A set of unused virgin polystyrene coffee cup lids were distributed in the environment (Sutton Bonington, UK) for a period of 24 months to compare monthly degradation rates across four treatments with variable degrees of exposure to natural UV irradiance (full or reduced exposure) and soil (surface...