Effect of Cr addition on the hot deformation behavior and microstructure evolution of Cu-0.8Fe-0.2Mg alloy
The Cu-0.8Fe-0.2Mg and Cu-0.8Fe-0.2Mg-0.2Cr alloys were investigated using hot compression experiments at 600–950 °C and 0.003–10 s−1 strain rates. The effects of Cr addition on the microstructure and recrystallized behavior of the Cu-0.8Fe-0.2Mg alloy were characterized by electron backscatter diff...