Optimizing Dielectric Constant in Tetragonal BaTiO3 Via Densification, Tetragonality, and Grain Growth Kinetic with Sintering Temperature
Tetragonal BaTiO3 nanopowders with tetragonality (c/a = 1.01), compacted uniaxially at 300 MPa, underwent sintering at temperatures ranging from 900°C to 1200°C for 1 h. Their densification and microstructure evolution were examined to determine the dielectric constant as a function of temperature (...
Saved in:
| Main Authors: | J. Lee, J. Jeong, J. Jung, H. Jeong |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Polish Academy of Sciences
2025-06-01
|
| Series: | Archives of Metallurgy and Materials |
| Subjects: | |
| Online Access: | https://journals.pan.pl/Content/135577/AMM-2025-2-26-Lee.pdf |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Sintering behaviour and dielectric properties of BaTiO3: Effect of borax addition
by: Othman Kolthoum I., et al.
Published: (2024-12-01) -
Subsurface State Bilayer in Tetragonal Ferroelectric BaTiO3
by: Junhao Chen, et al.
Published: (2025-06-01) -
Cold sintered BaTiO3–poly(ether imide) nanocomposites with superior comprehensive performances
by: Xinyi Li, et al.
Published: (2024-09-01) -
Sintering densification behavior of molybdenum tungsten alloys
by: WU Zhou, et al.
Published: (2021-06-01) -
Densification Behaviors of Zirconium Carbide with Silicon Additive Produced by Spark Plasma Sintering
by: Qisen Ren, et al.
Published: (2025-09-01)