Process window for manufacturing soft magnetic FeSi 6.5% by laser metal deposition
This study introduces Laser Metal Deposition (LMD) for the first time in manufacturing FeSi 6.5%, a crucial soft magnetic material. The investigation focuses on the impact of energy density on fabrication, emphasizing porosity, crack formation, and identifying an optimal processing window. Results r...
Saved in:
| Main Authors: | Karami Rasoul, Butler David, Javadi Yashar, Tamimi Saeed |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
EDP Sciences
2024-01-01
|
| Series: | MATEC Web of Conferences |
| Online Access: | https://www.matec-conferences.org/articles/matecconf/pdf/2024/13/matecconf_icmr2024_02011.pdf |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Ab Initio Study of the Conductivities of B2 FeSi Under Core‐Mantle Boundary Conditions
by: Yonghui Huang, et al.
Published: (2025-05-01) -
Room-temperature FeSi2-doped Cu2Se thermoelectric films with enhanced figure of merit
by: Masahiro Goto, et al.
Published: (2025-07-01) -
Numerical simulation of a highly efficient perovskite solar cell based on FeSi2 photoactive layer
by: George G. Njema, et al.
Published: (2024-09-01) -
Author Correction: Giant converse magnetoelectric effect in a multiferroic heterostructure with polycrystalline Co2FeSi
by: Shumpei Fujii, et al.
Published: (2024-10-01) -
Thermal stability of FeSi as barrier layer in high-performance Mg2Si0.3Sn0.7 thermoelectric device
by: Shanshan Hu, et al.
Published: (2025-09-01)