Synthesis, Chacterization, and Thermal Study of Terpolymeric Resin Derived from m-cresol, Hexamine and Formaldehyde

Terpolymeric resin was prepared from m-cresol (0.1M), hexamine (0.05M) and formaldehyde (0.2M) by acid catalyzed polycondensation method using 1M HCl in temperature range of 122-130°C.The resin was abbreviated as m-CHF-I. The molecular weight of terpolymer was determined by non-aqueous conductometri...

Full description

Saved in:
Bibliographic Details
Main Authors: K. M. Khedkar, V. V. Hiwase, A. B. Kalambe, S. D. Deosarkar
Format: Article
Language:English
Published: Wiley 2012-01-01
Series:E-Journal of Chemistry
Online Access:http://dx.doi.org/10.1155/2012/687860
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Terpolymeric resin was prepared from m-cresol (0.1M), hexamine (0.05M) and formaldehyde (0.2M) by acid catalyzed polycondensation method using 1M HCl in temperature range of 122-130°C.The resin was abbreviated as m-CHF-I. The molecular weight of terpolymer was determined by non-aqueous conductometric titration technique. The structure of resin was determined by its elemental analysis, UV-VIS, IR, and NMR data. The thermokinetic parameters were determined using Freeman-Carroll (FC) and Sharp Wentworth (SW) method in temperature range (410-485°C).The values of activation energies (Ea), entropy (∆S), and free energies (∆G) were in good agreement . The order of degradation reaction determined by FC method was confirmed by SW method.