Test on Discarding Tailings of Waste Rocks of a Vanadium-titanium Magnetite in Panxi Area
The combined methods of dry-discarding and wet-discarding were used to separate the vanadium-titanium-magnetite waste rock in Panxi. The results indicated that the grades of TFe and TiO2 which existed in the tailings reached 9.96% and 3.92%, respectively, and the recovery reached 23.73% using the dr...
Saved in:
| Main Authors: | , , , |
|---|---|
| Format: | Article |
| Language: | zho |
| Published: |
Institute of Multipurpose Utilization of Mineral Resources, Chinese Academy of Geological Sciences
2025-02-01
|
| Series: | Kuangchan zonghe liyong |
| Subjects: | |
| Online Access: | http://www.kczhly.com/en/article/doi/10.3969/j.issn.1000-6532.2025.01.024 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| _version_ | 1850229081559269376 |
|---|---|
| author | Jianping WANG Weiwei LI Deqiang LUO Xuehong WU |
| author_facet | Jianping WANG Weiwei LI Deqiang LUO Xuehong WU |
| author_sort | Jianping WANG |
| collection | DOAJ |
| description | The combined methods of dry-discarding and wet-discarding were used to separate the vanadium-titanium-magnetite waste rock in Panxi. The results indicated that the grades of TFe and TiO2 which existed in the tailings reached 9.96% and 3.92%, respectively, and the recovery reached 23.73% using the dry-discarding method after the waste rocks were crushed to -40 mm. In addition, after the concentrates of dry-discarding were crushed to -5 mm, using the wet-discarding method, the grades of TFe and TiO2 which existed in the tailings reached 7.86% and 2.81%, respectively, and the recovery reached 27.36%. Finally, the discarding rate reached 51.09% using the combination methods of dry-discarding and wet-discarding, and the TFe grade of concentrate increased 5.56 percentage, TiO2 grade increased 2.75 percentage. The method could greatly reduce the subsequent grinding amount, improve the initial grade, and reduce the mineral processing cost. |
| format | Article |
| id | doaj-art-bf71a8e55382407bb26bbdfc0d8c74f6 |
| institution | OA Journals |
| issn | 1000-6532 |
| language | zho |
| publishDate | 2025-02-01 |
| publisher | Institute of Multipurpose Utilization of Mineral Resources, Chinese Academy of Geological Sciences |
| record_format | Article |
| series | Kuangchan zonghe liyong |
| spelling | doaj-art-bf71a8e55382407bb26bbdfc0d8c74f62025-08-20T02:04:20ZzhoInstitute of Multipurpose Utilization of Mineral Resources, Chinese Academy of Geological SciencesKuangchan zonghe liyong1000-65322025-02-0146118118710.3969/j.issn.1000-6532.2025.01.0242025-01wangjianpingTest on Discarding Tailings of Waste Rocks of a Vanadium-titanium Magnetite in Panxi AreaJianping WANG0Weiwei LI1Deqiang LUO2Xuehong WU3Mining Company’s Designing Research Institute Panzhihua Steel, State Key Laboratory about Comprehensive Utilization of Vanadium Titanium Resources, Panzhihua 617063, Sichuan, ChinaMining Company’s Designing Research Institute Panzhihua Steel, State Key Laboratory about Comprehensive Utilization of Vanadium Titanium Resources, Panzhihua 617063, Sichuan, ChinaMining Company’s Designing Research Institute Panzhihua Steel, State Key Laboratory about Comprehensive Utilization of Vanadium Titanium Resources, Panzhihua 617063, Sichuan, ChinaMining Company’s Designing Research Institute Panzhihua Steel, State Key Laboratory about Comprehensive Utilization of Vanadium Titanium Resources, Panzhihua 617063, Sichuan, ChinaThe combined methods of dry-discarding and wet-discarding were used to separate the vanadium-titanium-magnetite waste rock in Panxi. The results indicated that the grades of TFe and TiO2 which existed in the tailings reached 9.96% and 3.92%, respectively, and the recovery reached 23.73% using the dry-discarding method after the waste rocks were crushed to -40 mm. In addition, after the concentrates of dry-discarding were crushed to -5 mm, using the wet-discarding method, the grades of TFe and TiO2 which existed in the tailings reached 7.86% and 2.81%, respectively, and the recovery reached 27.36%. Finally, the discarding rate reached 51.09% using the combination methods of dry-discarding and wet-discarding, and the TFe grade of concentrate increased 5.56 percentage, TiO2 grade increased 2.75 percentage. The method could greatly reduce the subsequent grinding amount, improve the initial grade, and reduce the mineral processing cost.http://www.kczhly.com/en/article/doi/10.3969/j.issn.1000-6532.2025.01.024mineral processing engineeringwasterocksdry-discardingwet-discarding |
| spellingShingle | Jianping WANG Weiwei LI Deqiang LUO Xuehong WU Test on Discarding Tailings of Waste Rocks of a Vanadium-titanium Magnetite in Panxi Area Kuangchan zonghe liyong mineral processing engineering wasterocks dry-discarding wet-discarding |
| title | Test on Discarding Tailings of Waste Rocks of a Vanadium-titanium Magnetite in Panxi Area |
| title_full | Test on Discarding Tailings of Waste Rocks of a Vanadium-titanium Magnetite in Panxi Area |
| title_fullStr | Test on Discarding Tailings of Waste Rocks of a Vanadium-titanium Magnetite in Panxi Area |
| title_full_unstemmed | Test on Discarding Tailings of Waste Rocks of a Vanadium-titanium Magnetite in Panxi Area |
| title_short | Test on Discarding Tailings of Waste Rocks of a Vanadium-titanium Magnetite in Panxi Area |
| title_sort | test on discarding tailings of waste rocks of a vanadium titanium magnetite in panxi area |
| topic | mineral processing engineering wasterocks dry-discarding wet-discarding |
| url | http://www.kczhly.com/en/article/doi/10.3969/j.issn.1000-6532.2025.01.024 |
| work_keys_str_mv | AT jianpingwang testondiscardingtailingsofwasterocksofavanadiumtitaniummagnetiteinpanxiarea AT weiweili testondiscardingtailingsofwasterocksofavanadiumtitaniummagnetiteinpanxiarea AT deqiangluo testondiscardingtailingsofwasterocksofavanadiumtitaniummagnetiteinpanxiarea AT xuehongwu testondiscardingtailingsofwasterocksofavanadiumtitaniummagnetiteinpanxiarea |