METAL RESEARCH OF THE REASONS OF BREAKAGE AT DRAWING OF ROLLED WIRE OF STEEL SV-08G2S
Metallurgical reasons of metal breakage at wire drawing, connected with microstructure of rolled wire, are examined.
Saved in:
| Main Authors: | A. M. Nesterenko, A. B. Sychkov, S. Ju. Zhukova |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Belarusian National Technical University
2011-02-01
|
| Series: | Литьë и металлургия |
| Online Access: | https://lim.bntu.by/jour/article/view/493 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
PECULIARITIES OF INFLUENCE OF MICROALLOYING WITH BORON ON STRAIN AGEING OF ROLLED WIRE OF STEEL SV-08G2S
by: A. M. Nesterenko, et al.
Published: (2010-09-01) -
PECULIARITIES OF INFLUENCE OF MICROALLOYING WITH BORON ON STRAIN AGEING OF ROLLED WIRE OF STEEL SV-08G2C
by: A. M. Nesterenko, et al.
Published: (2010-11-01) -
Experience in the production of wire rods made of steel grade SV‑08G2S for the subsequent manufacture of welding wire
by: S. V. Аudzeyey, et al.
Published: (2023-01-01) -
FORMATION OF SCALE PROPERTIES FOR ITS FULL REMOVAL FROM THE ROLLED WIRE SURFACE BEFORE WIRE DRAWING
by: A. B. Sychkov, et al.
Published: (2012-11-01) -
FORMING OF SCALE CHARACTERISTICS FOR ITS FULL ELIMINATION FROM THE ROLLED WIRE SURFACE BEFORE WIRE DRAWING
by: A. B. Sychkov, et al.