Effect of etching with different hydrofluoric acid concentrations on bond strength between glazed feldspathic ceramic and metal brackets

Objective – The aim of this study was evaluate the effect of etching with different hydrofluoric acid (HF) concentrations on the shear bond strength between glazed feldspathic ceramic and metal brackets. Materials and Methods – Seventy-five blocks of glazed feldspathic ceramic were produced and ran...

Full description

Saved in:
Bibliographic Details
Main Authors: Cristiane Frantz Arend, André Gundel, Renésio Armindo Grehs, Vilmar Antônio Ferrazzo, Luiz Felipe Valandro
Format: Article
Language:English
Published: Universidade Estadual Paulista 2016-03-01
Series:Brazilian Dental Science
Online Access:https://ojs.ict.unesp.br/index.php/cob/article/view/1193
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Objective – The aim of this study was evaluate the effect of etching with different hydrofluoric acid (HF) concentrations on the shear bond strength between glazed feldspathic ceramic and metal brackets. Materials and Methods – Seventy-five blocks of glazed feldspathic ceramic were produced and randomly allocated to 5 groups: Ctrl- silane application only; HF1- HF1%+silane; HF3- HF3%+silane; HF5- HF5%+silane; HF10- HF10%+silane (standard procedures:  etching for 1 min + washing + drying + silanization). Metal brackets for upper central incisors (Edgewise Standard) were bonded on the ceramic surface with the use of an adhesive system and light-cured composite resin (TransbondTM XT, 3M). The specimens were aged for 60 days (thermocycling: 10000x at 5-55 °C; stored in distilled water at 37 °C). Shear testing was performed, and specimens were classified for their Adhesive-Remnant-Index (ARI). Topographical inspection and contact angle analysis of the etched ceramic surfaces were performed. Data were statistically analyzed using the non-parametric Kruskal-Wallis test. One-way ANOVA and post-hoc Tukey’s tests were applied to the contact angle data (p < 0.05). Results – No significant difference was detected between the shear bond strength of the groups; but surface etching had a significant influence on the contact angle results (p < 0.00001). The control group presented the highest mean contact angle (61.8 ± 17.2°). All specimens showed adhesive failure at the resin-ceramic interface. Conclusion – The tested HF concentrations did not significantly influence the obtained shear bond strength of metal brackets adhered to glazed feldspathic ceramic surfaces. Keywords Ceramics; Hydrofluoric acid; Adhesion; Brackets; Silanization.
ISSN:2178-6011