A Study on Contact Fatigue Performance of Nitrided and TiN Coated Gears
This paper discusses the effects of TiN coating on gear contact fatigue performance through contact fatigue experiment and gear rig test. The results reveal that the deposition on gears with hard coating TiN could provide the subsurface protection and improve the contact fatigue life, and the contac...
Saved in:
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Wiley
2013-01-01
|
Series: | Advances in Materials Science and Engineering |
Online Access: | http://dx.doi.org/10.1155/2013/580470 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
_version_ | 1832562066089574400 |
---|---|
author | Hongbin Xu Hui Li Jianjun Hu Song Wang |
author_facet | Hongbin Xu Hui Li Jianjun Hu Song Wang |
author_sort | Hongbin Xu |
collection | DOAJ |
description | This paper discusses the effects of TiN coating on gear contact fatigue performance through contact fatigue experiment and gear rig test. The results reveal that the deposition on gears with hard coating TiN could provide the subsurface protection and improve the contact fatigue life, and the contact fatigue strength of nitrided+TiN coated 32Cr2MoV is 1557 MPa at survival probability of 99%, 284 MPa higher than that of nitrided 32Cr2MoV. Although TiN coating on the the edge of the meshing zone wore out, there is no obvious pitting at the site and the rest of meshed zone of TiN coated gear keeps well without pittings and wear grooves, which is opposite to nitrided gears with pittings and peeling off. TiN coating is dense and smooth with lower surface roughness, and it wraps up the gear tooth so that the gear surface no longer contacts with lubricant and prevents the cracks initiation, prolonging the contact fatigue life of gears. |
format | Article |
id | doaj-art-9b8d280a9b1741318b2cd759b2f603b4 |
institution | Kabale University |
issn | 1687-8434 1687-8442 |
language | English |
publishDate | 2013-01-01 |
publisher | Wiley |
record_format | Article |
series | Advances in Materials Science and Engineering |
spelling | doaj-art-9b8d280a9b1741318b2cd759b2f603b42025-02-03T01:23:37ZengWileyAdvances in Materials Science and Engineering1687-84341687-84422013-01-01201310.1155/2013/580470580470A Study on Contact Fatigue Performance of Nitrided and TiN Coated GearsHongbin Xu0Hui Li1Jianjun Hu2Song Wang3Key Laboratory of Manufacture and Test Techniques for Automobile Parts, Ministry of Education, Chongqing 400054, ChinaMaterial Science and Engineering College, Chongqing University of Technology, Chongqing 400054, ChinaMaterial Science and Engineering College, Chongqing University of Technology, Chongqing 400054, ChinaMaterial Science and Engineering College, Chongqing University of Technology, Chongqing 400054, ChinaThis paper discusses the effects of TiN coating on gear contact fatigue performance through contact fatigue experiment and gear rig test. The results reveal that the deposition on gears with hard coating TiN could provide the subsurface protection and improve the contact fatigue life, and the contact fatigue strength of nitrided+TiN coated 32Cr2MoV is 1557 MPa at survival probability of 99%, 284 MPa higher than that of nitrided 32Cr2MoV. Although TiN coating on the the edge of the meshing zone wore out, there is no obvious pitting at the site and the rest of meshed zone of TiN coated gear keeps well without pittings and wear grooves, which is opposite to nitrided gears with pittings and peeling off. TiN coating is dense and smooth with lower surface roughness, and it wraps up the gear tooth so that the gear surface no longer contacts with lubricant and prevents the cracks initiation, prolonging the contact fatigue life of gears.http://dx.doi.org/10.1155/2013/580470 |
spellingShingle | Hongbin Xu Hui Li Jianjun Hu Song Wang A Study on Contact Fatigue Performance of Nitrided and TiN Coated Gears Advances in Materials Science and Engineering |
title | A Study on Contact Fatigue Performance of Nitrided and TiN Coated Gears |
title_full | A Study on Contact Fatigue Performance of Nitrided and TiN Coated Gears |
title_fullStr | A Study on Contact Fatigue Performance of Nitrided and TiN Coated Gears |
title_full_unstemmed | A Study on Contact Fatigue Performance of Nitrided and TiN Coated Gears |
title_short | A Study on Contact Fatigue Performance of Nitrided and TiN Coated Gears |
title_sort | study on contact fatigue performance of nitrided and tin coated gears |
url | http://dx.doi.org/10.1155/2013/580470 |
work_keys_str_mv | AT hongbinxu astudyoncontactfatigueperformanceofnitridedandtincoatedgears AT huili astudyoncontactfatigueperformanceofnitridedandtincoatedgears AT jianjunhu astudyoncontactfatigueperformanceofnitridedandtincoatedgears AT songwang astudyoncontactfatigueperformanceofnitridedandtincoatedgears AT hongbinxu studyoncontactfatigueperformanceofnitridedandtincoatedgears AT huili studyoncontactfatigueperformanceofnitridedandtincoatedgears AT jianjunhu studyoncontactfatigueperformanceofnitridedandtincoatedgears AT songwang studyoncontactfatigueperformanceofnitridedandtincoatedgears |