LAJU OKSIDASI TITANIUM MURNI (CPTI GRADE TIPE 340) BERLAPIS HYDROXYAPATITE (HA) YANG DISINTER DALAM TUNGKU PERLAKUAN PANAS

<p>Implants are used for various reasons, such as replacing damaged tissue caused by disease or trauma, as filler and support the healing phase. The general terminology of biocompatibility describes a condition which will not cause harmful interaction between foreign material and the body. Bio...

Full description

Saved in:
Bibliographic Details
Main Authors: Desmarita Leni, Gunawarman Gunawarman, Jon Affi, Yuli Yetri
Format: Article
Language:English
Published: Department of Mechanical Engineering, Faculty of Engineering, Universitas Andalas 2019-07-01
Series:Metal: Jurnal Sistem Mekanik dan Termal
Subjects:
Online Access:https://metal.ft.unand.ac.id/index.php/metal/article/view/78
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1832574963454836736
author Desmarita Leni
Gunawarman Gunawarman
Jon Affi
Yuli Yetri
author_facet Desmarita Leni
Gunawarman Gunawarman
Jon Affi
Yuli Yetri
author_sort Desmarita Leni
collection DOAJ
description <p>Implants are used for various reasons, such as replacing damaged tissue caused by disease or trauma, as filler and support the healing phase. The general terminology of biocompatibility describes a condition which will not cause harmful interaction between foreign material and the body. Biocompatibility is a system  including physical, chemical, biological, medical, and design aspects. This study is focused on the influence of the coating thickness of hidroxyapatite layer on the rate of oxidation. Pure titanium  coated by HA with thickness variation needs to be tested for oxidation resistance to determine the  coating effectiveness in reducing the rate of oxidation. The rate of oxidation  measured by weight loss method after coated titanium by HA and than heating in a heat furnance. HA coatings obtained by a process of electrophoretic deposition (EPD) with  variation of time between  5 to 35 minutes at a voltage of 40 V with fineness of 30 µm. The oxidation process was done during the sintering process in a heat furnace for 10 minutes. The result of this study shows that the increase of time EPD increases the thickness of HA layer. Oxidation resistance on CPTi after HA coating does not cause the quality of pure titanium degraded in addition,  the oxidation resistance of HA increases from good grade to excellent grade. It shows that the formation of surface oxide slows down during sintering process.</p>
format Article
id doaj-art-89fba3a6039c4ea3abafa0e1cc11442e
institution Kabale University
issn 2598-1137
2597-4483
language English
publishDate 2019-07-01
publisher Department of Mechanical Engineering, Faculty of Engineering, Universitas Andalas
record_format Article
series Metal: Jurnal Sistem Mekanik dan Termal
spelling doaj-art-89fba3a6039c4ea3abafa0e1cc11442e2025-02-01T10:20:39ZengDepartment of Mechanical Engineering, Faculty of Engineering, Universitas AndalasMetal: Jurnal Sistem Mekanik dan Termal2598-11372597-44832019-07-0131465010.25077/metal.3.1.46-50.201945LAJU OKSIDASI TITANIUM MURNI (CPTI GRADE TIPE 340) BERLAPIS HYDROXYAPATITE (HA) YANG DISINTER DALAM TUNGKU PERLAKUAN PANASDesmarita Leni0Gunawarman Gunawarman1Jon Affi2Yuli Yetri3Sekolah Menengah Kejuruan Semen PadangUniversitas AndalasUniversitas AndalasPoliteknik Negeri Padang<p>Implants are used for various reasons, such as replacing damaged tissue caused by disease or trauma, as filler and support the healing phase. The general terminology of biocompatibility describes a condition which will not cause harmful interaction between foreign material and the body. Biocompatibility is a system  including physical, chemical, biological, medical, and design aspects. This study is focused on the influence of the coating thickness of hidroxyapatite layer on the rate of oxidation. Pure titanium  coated by HA with thickness variation needs to be tested for oxidation resistance to determine the  coating effectiveness in reducing the rate of oxidation. The rate of oxidation  measured by weight loss method after coated titanium by HA and than heating in a heat furnance. HA coatings obtained by a process of electrophoretic deposition (EPD) with  variation of time between  5 to 35 minutes at a voltage of 40 V with fineness of 30 µm. The oxidation process was done during the sintering process in a heat furnace for 10 minutes. The result of this study shows that the increase of time EPD increases the thickness of HA layer. Oxidation resistance on CPTi after HA coating does not cause the quality of pure titanium degraded in addition,  the oxidation resistance of HA increases from good grade to excellent grade. It shows that the formation of surface oxide slows down during sintering process.</p>https://metal.ft.unand.ac.id/index.php/metal/article/view/78hydroxyapatite comercial pure titanium weight loss sintering.
spellingShingle Desmarita Leni
Gunawarman Gunawarman
Jon Affi
Yuli Yetri
LAJU OKSIDASI TITANIUM MURNI (CPTI GRADE TIPE 340) BERLAPIS HYDROXYAPATITE (HA) YANG DISINTER DALAM TUNGKU PERLAKUAN PANAS
Metal: Jurnal Sistem Mekanik dan Termal
hydroxyapatite comercial pure titanium weight loss sintering.
title LAJU OKSIDASI TITANIUM MURNI (CPTI GRADE TIPE 340) BERLAPIS HYDROXYAPATITE (HA) YANG DISINTER DALAM TUNGKU PERLAKUAN PANAS
title_full LAJU OKSIDASI TITANIUM MURNI (CPTI GRADE TIPE 340) BERLAPIS HYDROXYAPATITE (HA) YANG DISINTER DALAM TUNGKU PERLAKUAN PANAS
title_fullStr LAJU OKSIDASI TITANIUM MURNI (CPTI GRADE TIPE 340) BERLAPIS HYDROXYAPATITE (HA) YANG DISINTER DALAM TUNGKU PERLAKUAN PANAS
title_full_unstemmed LAJU OKSIDASI TITANIUM MURNI (CPTI GRADE TIPE 340) BERLAPIS HYDROXYAPATITE (HA) YANG DISINTER DALAM TUNGKU PERLAKUAN PANAS
title_short LAJU OKSIDASI TITANIUM MURNI (CPTI GRADE TIPE 340) BERLAPIS HYDROXYAPATITE (HA) YANG DISINTER DALAM TUNGKU PERLAKUAN PANAS
title_sort laju oksidasi titanium murni cpti grade tipe 340 berlapis hydroxyapatite ha yang disinter dalam tungku perlakuan panas
topic hydroxyapatite comercial pure titanium weight loss sintering.
url https://metal.ft.unand.ac.id/index.php/metal/article/view/78
work_keys_str_mv AT desmaritaleni lajuoksidasititaniummurnicptigradetipe340berlapishydroxyapatitehayangdisinterdalamtungkuperlakuanpanas
AT gunawarmangunawarman lajuoksidasititaniummurnicptigradetipe340berlapishydroxyapatitehayangdisinterdalamtungkuperlakuanpanas
AT jonaffi lajuoksidasititaniummurnicptigradetipe340berlapishydroxyapatitehayangdisinterdalamtungkuperlakuanpanas
AT yuliyetri lajuoksidasititaniummurnicptigradetipe340berlapishydroxyapatitehayangdisinterdalamtungkuperlakuanpanas