Ultra-Short-Pulse Laser Welding of Glass to Metal with a Shear Strength Above 50 MPa
We report an ultra-short-pulse laser welding process that allows one to consistently weld Borofloat<sup>®</sup> 33 glass to aluminum with a shear strength above 50 MPa. We explored the morphology of the welding seam and quantified the quality of the bonding by statistically determining t...
Saved in:
| Main Authors: | Lukas Günther, Jens Ulrich Thomas, Jens Hermann, Axel Ohlinger, Dominique de Ligny |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
MDPI AG
2025-04-01
|
| Series: | Micromachines |
| Subjects: | |
| Online Access: | https://www.mdpi.com/2072-666X/16/5/538 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Direct Glass-to-Metal Welding by Femtosecond Laser Pulse Bursts: I, Conditions for Successful Welding with a Gap
by: Qingfeng Li, et al.
Published: (2025-08-01) -
Process characteristics of thick flux band-constrained arc ultra-narrow gap welding method
by: Zhenmin LIU, et al.
Published: (2025-08-01) -
Modification of the materials of the welded zone in the ultra‑deep penetration mode
by: Yu. S. Usherenko, et al.
Published: (2022-05-01) -
Retained austenite in multipass high-strength weld metal with a yield strength exceeding 1100 MPa
by: Daniel Schrittwieser, et al.
Published: (2025-05-01) -
Femtosecond laser photochemical reduction of silver ion solution for micro-welding of transparent and hard materials for solar cell packaging
by: Hao Chen, et al.
Published: (2025-08-01)