Changes in performance and thermal stability of Ni0.8Co0.1Al0.1/graphite batteries with excessive water
Abstract During the production process of lithium‐ion batteries, there exists a scenario of excessive water inside the battery due to poor water control in the factory environment. In addition, the battery housing may be damaged by corrosion, external vibration etc., which would cause water to enter...
Saved in:
| Main Authors: | Xi Liu, Jingbo Mao, Hongtao Yan, Chunjing Lin, Chuang Qi, Tao Yan, Li Lao, Yazhou Sun |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Wiley
2024-12-01
|
| Series: | IET Energy Systems Integration |
| Subjects: | |
| Online Access: | https://doi.org/10.1049/esi2.12148 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Norbornenic anhydride as versatile additive optimizing interphases to enable high-performance LiNi0.8Co0.1Mn0.1O2/Li batteries
by: Fujie Yang, et al.
Published: (2025-04-01) -
Synthesis of nano cubic microstructure LiNi0.8Co0.1Mn0.1O2 cathode materials via rapid precipitation assisted with hydrothermal treatment
by: Jing Lao, et al.
Published: (2024-11-01) -
Analysis of Degradation Mechanisms in LiNi0.8Mn0.1Co0.1O2 Lithium-ion Battery Cathodes During High-Rate Charge–Discharge Cycling
by: Daisuke SHIBATA, et al.
Published: (2025-06-01) -
Fly-ash derived crystalline Si (cSi) Improves the capacity and energy density of LiNi0.8Co0.1Mn0.1O2 battery: Synthesis and performance
by: Cornelius Satria Yudha, et al.
Published: (2024-12-01) -
An overview on the structure and electrochemical properties of Co-free Ni-rich LiNi0.8Mn0.1Fe0.1O2 as a cathode material for lithium-ion batteries
by: Rasha S. El-Tawil, et al.
Published: (2025-08-01)