Formability, Mechanical and Chemical Properties Assessment for High Strength AA7075 Subjected to Annealing Heat Treatment
The current study examined how the annealing process affected the formability, mechanical and chemical characteristics of 7075 alloy. The formability was achieved during the bending test. Tensile, hardness, microstructure and corrosion tests represent mechanical and chemical properties. The test sp...
Saved in:
Main Authors: | , , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
middle technical university
2023-03-01
|
Series: | Journal of Techniques |
Subjects: | |
Online Access: | https://journal.mtu.edu.iq/index.php/MTU/article/view/1107 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
_version_ | 1832595117554270208 |
---|---|
author | Naseer Malik Abbas Zahraa Thamer Abdulwahid Asmaa Ali Hussien S.V. Konovalov Hamid M. Mahan |
author_facet | Naseer Malik Abbas Zahraa Thamer Abdulwahid Asmaa Ali Hussien S.V. Konovalov Hamid M. Mahan |
author_sort | Naseer Malik Abbas |
collection | DOAJ |
description |
The current study examined how the annealing process affected the formability, mechanical and chemical characteristics of 7075 alloy. The formability was achieved during the bending test. Tensile, hardness, microstructure and corrosion tests represent mechanical and chemical properties. The test specimens for each test were prepared then followed by annealing heat treatment by heating them to 200 and 300°C in an electrical furnace for two hours. Then, the specimens were allowed to cool in the furnace to a room temperature. The results indicate that the tensile strength and hardness were decreased for about 50%. Bending strength was increased by approximately 30%, where the specimens bent at a very high angle without cracking or breaking in comparison to base metal. Annealing heat treatment with a proper selected procedures and temperatures was able to stabilize the microstructure and release the second phase precipitate particles. Annealing process contributed in improving formability, ductility and corrosion resistance of the Al 7075 alloy.
|
format | Article |
id | doaj-art-5aef6cc121bc458d8c1161f077b9bf9b |
institution | Kabale University |
issn | 1818-653X 2708-8383 |
language | English |
publishDate | 2023-03-01 |
publisher | middle technical university |
record_format | Article |
series | Journal of Techniques |
spelling | doaj-art-5aef6cc121bc458d8c1161f077b9bf9b2025-01-19T11:01:57Zengmiddle technical universityJournal of Techniques1818-653X2708-83832023-03-015110.51173/jt.v5i1.1107Formability, Mechanical and Chemical Properties Assessment for High Strength AA7075 Subjected to Annealing Heat TreatmentNaseer Malik Abbas0Zahraa Thamer Abdulwahid1Asmaa Ali Hussien2S.V. Konovalov3Hamid M. Mahan4Institute of Technology / Baghdad, Middle Technical University, Baghdad, IraqInstitute of Technology / Baghdad, Middle Technical University, Baghdad, IraqInstitute of Medical Technology / Mansour, Middle Technical University, Baghdad, IraqSiberian State Industrial University, Kirov str., 42, 654007, Novokuznetsk, RussiaSamara National Research University, Moskovskoye road, 34, 443086, Samara, Russia The current study examined how the annealing process affected the formability, mechanical and chemical characteristics of 7075 alloy. The formability was achieved during the bending test. Tensile, hardness, microstructure and corrosion tests represent mechanical and chemical properties. The test specimens for each test were prepared then followed by annealing heat treatment by heating them to 200 and 300°C in an electrical furnace for two hours. Then, the specimens were allowed to cool in the furnace to a room temperature. The results indicate that the tensile strength and hardness were decreased for about 50%. Bending strength was increased by approximately 30%, where the specimens bent at a very high angle without cracking or breaking in comparison to base metal. Annealing heat treatment with a proper selected procedures and temperatures was able to stabilize the microstructure and release the second phase precipitate particles. Annealing process contributed in improving formability, ductility and corrosion resistance of the Al 7075 alloy. https://journal.mtu.edu.iq/index.php/MTU/article/view/1107FormabilityMechanical PropertiesAnnealing Heat TreatmentCorrosion Test |
spellingShingle | Naseer Malik Abbas Zahraa Thamer Abdulwahid Asmaa Ali Hussien S.V. Konovalov Hamid M. Mahan Formability, Mechanical and Chemical Properties Assessment for High Strength AA7075 Subjected to Annealing Heat Treatment Journal of Techniques Formability Mechanical Properties Annealing Heat Treatment Corrosion Test |
title | Formability, Mechanical and Chemical Properties Assessment for High Strength AA7075 Subjected to Annealing Heat Treatment |
title_full | Formability, Mechanical and Chemical Properties Assessment for High Strength AA7075 Subjected to Annealing Heat Treatment |
title_fullStr | Formability, Mechanical and Chemical Properties Assessment for High Strength AA7075 Subjected to Annealing Heat Treatment |
title_full_unstemmed | Formability, Mechanical and Chemical Properties Assessment for High Strength AA7075 Subjected to Annealing Heat Treatment |
title_short | Formability, Mechanical and Chemical Properties Assessment for High Strength AA7075 Subjected to Annealing Heat Treatment |
title_sort | formability mechanical and chemical properties assessment for high strength aa7075 subjected to annealing heat treatment |
topic | Formability Mechanical Properties Annealing Heat Treatment Corrosion Test |
url | https://journal.mtu.edu.iq/index.php/MTU/article/view/1107 |
work_keys_str_mv | AT naseermalikabbas formabilitymechanicalandchemicalpropertiesassessmentforhighstrengthaa7075subjectedtoannealingheattreatment AT zahraathamerabdulwahid formabilitymechanicalandchemicalpropertiesassessmentforhighstrengthaa7075subjectedtoannealingheattreatment AT asmaaalihussien formabilitymechanicalandchemicalpropertiesassessmentforhighstrengthaa7075subjectedtoannealingheattreatment AT svkonovalov formabilitymechanicalandchemicalpropertiesassessmentforhighstrengthaa7075subjectedtoannealingheattreatment AT hamidmmahan formabilitymechanicalandchemicalpropertiesassessmentforhighstrengthaa7075subjectedtoannealingheattreatment |