Influence of Deposition Condition on Y2O3 Coatings Produced by Pulsed Electrophoretic Deposition
Y2O3 nanoparticle suspension aqueous solution was prepared using citric acid. Then, Y2O3 film was deposited using this solution with pulsed electrophoretic deposition (EPD). A dense Y2O3 film of 25.7 μm thickness was obtained with deposition conditions of 0.5 wt% Y2O3 concentration, bias voltage of...
Saved in:
| Main Authors: | Hidetoshi Miyazaki, Asumi Ichikawa, Hisao Suzuki, Toshitaka Ota |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Wiley
2016-01-01
|
| Series: | Advances in Materials Science and Engineering |
| Online Access: | http://dx.doi.org/10.1155/2016/9387651 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Understanding the structural and electrochemical properties of YSZ coating deposited by electrophoretic deposition
by: Omid Sharifahmadian, et al.
Published: (2025-06-01) -
Graphene reinforced hydroxyapatite biocomposite coatings obtained by electrophoretic deposition on titanium
by: Marija Đošić, et al.
Published: (2018-06-01) -
Variables Affecting Developments of Hydroxyapatite Coating by Using Electrophoretic Deposition Technique
by: Baghdad Science Journal
Published: (2008-09-01) -
Electrophoretic deposition of coatings and bulk compacts using magnesium-doped aluminum oxide nanopowders
by: E. G. Kalinina, et al.
Published: (2021-05-01) -
Synthesis and Characterization of Composite Coating of Iron Oxide and Bioactive Glass, Coated by Electrophoretic co-Deposition Method for Biomedical Applications
by: M. S. Abbasi, et al.
Published: (2023-08-01)