Studying The Optical Properties of CdO and CdO: Bi Thin Films
Cadmium Oxide and Bi doped Cadmium Oxide thin films are prepared by using the chemical spray pyrolysis technique a glass substrate at a temperature of (400?C) with volumetric concentration (2,4)%. The thickness of all prepared films is about (400±20) nm. Transmittance and Absorbance spectra are reco...
Saved in:
| Main Author: | |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
University of Baghdad, College of Science for Women
2016-09-01
|
| Series: | مجلة بغداد للعلوم |
| Subjects: | |
| Online Access: | http://bsj.uobaghdad.edu.iq/index.php/BSJ/article/view/2303 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Summary: | Cadmium Oxide and Bi doped Cadmium Oxide thin films are prepared by using the chemical spray pyrolysis technique a glass substrate at a temperature of (400?C) with volumetric concentration (2,4)%. The thickness of all prepared films is about (400±20) nm. Transmittance and Absorbance spectra are recorded in the wave length ranged (400-800) nm. The nature of electronic transitions is determined, it is found out that these films have directly allowed transition with an optical energy gap of (2.37( eV for CdO and ) 2.59, 2.62) eV for (2% ,4%) Bi doped CdO respectively. The optical constants have been evaluated before and after doping. |
|---|---|
| ISSN: | 2078-8665 2411-7986 |