HARDENING OF CASTINGS AT FREE FORMING OF INTERNAL SURFACE
The reasons of arising of the hollow castings polythickness at free forming of internal surface are investigated. The recommendations on its reduction are given
Saved in:
| Main Authors: | E. I. Marukovich, V. F. Bevza, V. P. Grusha |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Belarusian National Technical University
2005-08-01
|
| Series: | Литьë и металлургия |
| Online Access: | https://lim.bntu.by/jour/article/view/1882 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
LONGITUDINAL DIFFERENT-WALL OF HOLLOW CASTINGS AT FORMING OF INTERNAL SURFACE OUT OF MELT WITHOUT APPLICATION OF ROD
by: E. I. Marukovich, et al.
Published: (2006-05-01) -
FORMING OF HOLLOW SLUGS OF CAST IRON WITH GLOBULAR GRAPHITE IN CONDITIONS OF WALL CRYSTALLIZATIO
by: V. F. Bevza, et al.
Published: (2009-08-01) -
THERMAL DEFORMATION CONDITIONS FOR THE FORMATION OF HOLLOW CYLINDRICAL CAST IRON CASTING IN THE METAL WATER-COOLED FORM
by: E. I. Marukovich, et al.
Published: (2013-09-01) -
CONTINUOUSLY-CYCLIC CASTING OF HOLLOW CYLINDER SLUGS OF HIGH-CHROMIUM CAST IRON
by: E. I. Marukovich, et al.
Published: (2009-08-01) -
PRINCIPALLY NEW EFFECTIVE CASTING PROCESS OF THE HOLLOW CYLINDRICAL SLUGS OF CAST IRON BY METHOD OF DIRECTIONAL SOLIDIFICATION
by: E. I. Marukovich, et al.
Published: (2010-08-01)