EXFOLIATION AT WIRE TWISTING FOR TIRES BEAD RINGS
It is shown that reduction of twisting numbers up to destruction of cold drawn wire for bead rings is stipulated by junction of microcracks formed in longitudinallyand transverse-oriented planes of deformation shift with creation of main crack.
Saved in:
| Main Authors: | A. N. Savenok, A. V. Demidov, Ju. D. Gubanov, E. S. Seregina |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Belarusian National Technical University
2010-08-01
|
| Series: | Литьë и металлургия |
| Online Access: | https://lim.bntu.by/jour/article/view/872 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
CREATION OF THE CLASSIFIER OF BREAKS OF DRAWN WIRE OF THE STEEL WITH PEARLITE STRUCTURE AFTER TESTS ON TWISTING
by: E. S. Seregina
Published: (2007-02-01) -
CHOICE OF TECHNOLOGICAL PARAMETERS FOR PRODUCTION OF WIRE FOR ONBOARD RINGS WITH HEIGHTENED REQUIREMENTS TO ADHESION
by: A. V. Demidov, et al.
Published: (2012-11-01) -
STRUCTURE AND CHARACTERISTICS OF PATENTED HIGH-CARBON WIRE
by: A. Ju. Borisenko, et al.
Published: (2011-02-01) -
Improved Recovery of Exfoliated Colonocytes from Feces Using Newly Developed Immunomagnetic Beads
by: Yoshikatsu Koga, et al.
Published: (2008-01-01) -
DECREASE OF BREAKAGE OF HIGH-STRENGTH WIRE AT TWIST OF METAL CORD FROM IT ON CARS OF DOUBLE TORSION
by: V. A. Birukov, et al.
Published: (2012-05-01)