Determination of Crack Resistance of the Cover and Slide Glass by Indentation Method with the Visualization Using Atomic Force Microscopy
Crack resistance of two types of glass was studied – cover glass (0.17 mm thick) and slide glass (2 mm thick) using an improved technique through the use of the probe methods, which makes it possible to increase the accuracy of determining the crack resistance of glass. Colorless silicate glass was...
Saved in:
Main Authors: | , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Belarusian National Technical University
2024-04-01
|
Series: | Приборы и методы измерений |
Subjects: | |
Online Access: | https://pimi.bntu.by/jour/article/view/859 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
_version_ | 1832546374960283648 |
---|---|
author | V. A. Lapitskaya T. A. Kuznetsova S. A. Chizhik |
author_facet | V. A. Lapitskaya T. A. Kuznetsova S. A. Chizhik |
author_sort | V. A. Lapitskaya |
collection | DOAJ |
description | Crack resistance of two types of glass was studied – cover glass (0.17 mm thick) and slide glass (2 mm thick) using an improved technique through the use of the probe methods, which makes it possible to increase the accuracy of determining the crack resistance of glass. Colorless silicate glass was used. Crack resistance was determined by the Vickers pyramid indentation method. Microstructure of glasses surface and deformation region after indentation were studied using an atomic force microscope. Mechanical properties of glasses were determined by nanoindentation. Surface relief of a glass slide is rougher than that one of a cover glass. Roughness Rz for a cover glass is less than for a slide glass. Specific surface energy value of 0.26 N/m is higher for the slide glass compared to the coverslip. One elastic modulus value E of the cover glass is 48 GPa, and that one of the slide glass is 58 GPa. The microhardness value H is almost the same for by the glasses and amounts to 6.7 GPa for a slide glass and 6.4 GPa for a cover glass. Atomic force microscope images of deformation region after indentation with a Vickers pyramid show that the first cracks appear at a load of 1 N on the slide glass, and at 2 N on the cover glass. At a load of 3 N, the cover glass is destroyed. Based on the results of crack resistance calculations it was found that critical stress intensity coefficient KIC values are 1.42 MPa∙m1/2 for a glass slide, and 1.10 MPa∙m1/2 for a cover glass. |
format | Article |
id | doaj-art-0586d58071f140ab9e5a28d6a4e01e52 |
institution | Kabale University |
issn | 2220-9506 2414-0473 |
language | English |
publishDate | 2024-04-01 |
publisher | Belarusian National Technical University |
record_format | Article |
series | Приборы и методы измерений |
spelling | doaj-art-0586d58071f140ab9e5a28d6a4e01e522025-02-03T07:11:13ZengBelarusian National Technical UniversityПриборы и методы измерений2220-95062414-04732024-04-01151606710.21122/2220-9506-2024-15-1-60-67639Determination of Crack Resistance of the Cover and Slide Glass by Indentation Method with the Visualization Using Atomic Force MicroscopyV. A. Lapitskaya0T. A. Kuznetsova1S. A. Chizhik2A.V. Luikov Heat and Mass Transfer Institute of the National Academy of Science of Belarus; Belarusian National Technical UniversityA.V. Luikov Heat and Mass Transfer Institute of the National Academy of Science of Belarus; Belarusian National Technical UniversityA.V. Luikov Heat and Mass Transfer Institute of the National Academy of Science of Belarus; Belarusian National Technical UniversityCrack resistance of two types of glass was studied – cover glass (0.17 mm thick) and slide glass (2 mm thick) using an improved technique through the use of the probe methods, which makes it possible to increase the accuracy of determining the crack resistance of glass. Colorless silicate glass was used. Crack resistance was determined by the Vickers pyramid indentation method. Microstructure of glasses surface and deformation region after indentation were studied using an atomic force microscope. Mechanical properties of glasses were determined by nanoindentation. Surface relief of a glass slide is rougher than that one of a cover glass. Roughness Rz for a cover glass is less than for a slide glass. Specific surface energy value of 0.26 N/m is higher for the slide glass compared to the coverslip. One elastic modulus value E of the cover glass is 48 GPa, and that one of the slide glass is 58 GPa. The microhardness value H is almost the same for by the glasses and amounts to 6.7 GPa for a slide glass and 6.4 GPa for a cover glass. Atomic force microscope images of deformation region after indentation with a Vickers pyramid show that the first cracks appear at a load of 1 N on the slide glass, and at 2 N on the cover glass. At a load of 3 N, the cover glass is destroyed. Based on the results of crack resistance calculations it was found that critical stress intensity coefficient KIC values are 1.42 MPa∙m1/2 for a glass slide, and 1.10 MPa∙m1/2 for a cover glass.https://pimi.bntu.by/jour/article/view/859cover glassslide glasscrack resistanceindentation methodatomic force microscopy |
spellingShingle | V. A. Lapitskaya T. A. Kuznetsova S. A. Chizhik Determination of Crack Resistance of the Cover and Slide Glass by Indentation Method with the Visualization Using Atomic Force Microscopy Приборы и методы измерений cover glass slide glass crack resistance indentation method atomic force microscopy |
title | Determination of Crack Resistance of the Cover and Slide Glass by Indentation Method with the Visualization Using Atomic Force Microscopy |
title_full | Determination of Crack Resistance of the Cover and Slide Glass by Indentation Method with the Visualization Using Atomic Force Microscopy |
title_fullStr | Determination of Crack Resistance of the Cover and Slide Glass by Indentation Method with the Visualization Using Atomic Force Microscopy |
title_full_unstemmed | Determination of Crack Resistance of the Cover and Slide Glass by Indentation Method with the Visualization Using Atomic Force Microscopy |
title_short | Determination of Crack Resistance of the Cover and Slide Glass by Indentation Method with the Visualization Using Atomic Force Microscopy |
title_sort | determination of crack resistance of the cover and slide glass by indentation method with the visualization using atomic force microscopy |
topic | cover glass slide glass crack resistance indentation method atomic force microscopy |
url | https://pimi.bntu.by/jour/article/view/859 |
work_keys_str_mv | AT valapitskaya determinationofcrackresistanceofthecoverandslideglassbyindentationmethodwiththevisualizationusingatomicforcemicroscopy AT takuznetsova determinationofcrackresistanceofthecoverandslideglassbyindentationmethodwiththevisualizationusingatomicforcemicroscopy AT sachizhik determinationofcrackresistanceofthecoverandslideglassbyindentationmethodwiththevisualizationusingatomicforcemicroscopy |